Rich, are you of the opinion that gettering is a false concept?
In any case, 1400 deg C seems be to mighty hot (white hot?)

Ian ZS6BTE

measures wrote:
> 
> >
> >> >The 3-500Z getters itself through a Zirconium coating on the anode. This
> >> >is the coating that gives the anode a dull powdery gray color. Zirconium
> >> >absorbs different gases at different temperatures, with optimum gettering
> >> >for most gases occurring around 1400 degrees C. Optimum absorbing of
> >> >hydrogen occurs at 350 degrees C.
> >> ______________________________________________________________
> >>
> >> Very interesting.  Is there a similar effect with the graphite-anode
> >> versions?
> >>
> >> 73, Bill W7TI
> >
> >The effect is the same. The same materials are used.
> >
> Taurine feculence.
> 
> 
> >Graphite tends to release more gas and other impurities more than
> >hard metals, but otherwise gettering operation is about the same.
> 
>   Graphite anodes contain only graphite.  Graphite has the ability store
> gas, however, it does not getter. //  To feed their egos, some people
> fabricate.
> 
> end
> 
> -  Rich..., 805.386.3734, www.vcnet.com/measures.
> end

--
FAQ on WWW:               http://www.contesting.com/FAQ/amps
Submissions:              amps@contesting.com
Administrative requests:  amps-REQUEST@contesting.com
Problems:                 owner-amps@contesting.com


<Prev in Thread] Current Thread [Next in Thread>