ORIGINAL MESSAGE:
On Fri, 14 Jul 2006 08:16:20 -0700, you wrote:
>A company I used to work for used a "Hard Anodizing Process" for Aluminium
>transfer chutes in the food industry, this lasted pretty much for ever
>exposed to all sorts of chemicals, solvents and water. It was not a cheap
>process though.
------------ REPLY SEPARATOR ------------
As I understand it, anodizing leaves the surface non-conductive,
unlike chromate conversion. This might be ok for radials, however.
Bill, W6WRT