The advantage of silver soldering is that it happens at around red heat, and 
you're less likely to get burning of the copper or steel. The last issue of NCJ 
had a good article on silver soldering, although there were a few points not 
covered. The flux used can be something as simple as household borax made into 
a thick paste with water, although I use a commercial flux called 'Easyflow', 
which you mix with water to a thick paste. Silver solder, depending on which 
one you get, flows at between 600C and 700C.. the NCJ article said you mustn't 
have a gap: in fact, you need a gap between the materials being joined of 
between 2 and 8 thousandths of an inch, depending which silver solder you are 
using. The UK 'Easyflo #1' melts atbout 610C and needs a gap of about 1 to 2 
thousandths of an inch.
As others have said, for silver soldering, make sure everything is as clean as 
for soft soldering - no grease from fingers! - and use lots of flux. You 
usually find that the excess flux  comes off easily by pouring some cold water 
over the joint - for small copper locomotive boilers, it's not unusual to 
pickle in dilute sulphuric acid, but that's a bit OTT for this application!
Incidentally, mixing the flux is like mixing epoxy - you can only get two 
quantities - too much or too little! Too much is preferred....

73
Peter G3RZP
_______________________________________________



_______________________________________________
TowerTalk mailing list
TowerTalk@contesting.com
http://lists.contesting.com/mailman/listinfo/towertalk

<Prev in Thread] Current Thread [Next in Thread>