WS6X wrote:

>I am intrigued by the glowing TT comments regarding cold galvanizing spray. 
>Since my experience is so much to the contrary, I must be &#8220;Ralphing 
>up&#8221; the process somehow. I&#8217;m hoping someone here can correct the 
>error of my ways.
>
>I have tried 3 different brands. I have enthusiastically read all the promo 
>stuff: &#8220;Rich with self-sacrificing zinc, creating a durable bond, etc., 
>etc.&#8221;
>
>I have applied the spray paint directly over clean, existing galvanized steel. 
>I have applied it to new, buffed (with steel wool, and/or emery cloth) steel, 
>and to chemically etched, new steel. I have allowed it to &#8220;cure&#8221; 
>for 12 weeks. I have yet to achieve what I would consider a 
>&#8220;bond.&#8221; To wit: the paint can be scraped off down to original 
>surface with the slightest effort. In fact I can even rub it off with a callus 
>on my thumb!
>
>What am I missing?
>
>Thanks,
>
>Jim - WS6X

You only tried three brands? :-) I tried a dozen or so before
finding a good one.

Try "Brite Zinc".

It's leaves the hardest, best looking finish I've seen.

--
Steve K8LX


-----
FAQ on WWW:               http://www.contesting.com/FAQ/towertalk
Submissions:              towertalk@contesting.com
Administrative requests:  towertalk-REQUEST@contesting.com
Problems:                 owner-towertalk@contesting.com


<Prev in Thread] Current Thread [Next in Thread>