At 01:18 PM 12/24/2002 -0600, Paul DeWitte K9OT wrote: >Since schedule 80 is twice as thich as schedule 40 they are not the same >strength. Yield strength is a materials spec. Both Schedule 80 and 40 are the same material--so their material yield strength is the same. But the actual load they can handle is a function not only of the material yield strength but also the wall thickness and diameter. You need all three to calculate the capabilty of a mast. |