I wanted to make several Cadweld-type connections (#4 copper wire to 5/8 
inch ground rod) for my tower ground system, and I since I had already 
obtained a bunch of the weld metal powder on eBay I wanted to use a 
standard graphite mold instead of buying a bunch of One-Shots.  Not 
knowing my way around the industrial websites (and not wanting to set up 
a commercial account just for that purpose) I decided to try to 
fabricate my own mold.  The result may look a bit clumsy but it works.  
For the non-squeamish, details can be viewed at:

http://www.ab7e.com/exothermic/AB7E_Homebrew_Exothermic_Mold.html

73,
Dave   AB7E


_______________________________________________



_______________________________________________
TowerTalk mailing list
TowerTalk@contesting.com
http://lists.contesting.com/mailman/listinfo/towertalk

<Prev in Thread] Current Thread [Next in Thread>
  • [TowerTalk] Homebrew Exothermic Mold, David Gilbert <=