if they deterioate the plastic parts so fast am i not having probs???
tx de w7gg

----------
> From: Roger A. Cox WB0DGF <hygain@compuserve.com>
> To: Bob Wruble <ai7b@teleport.com>
> Cc: towertalk <towertalk@contesting.com>
> Subject: Re: [TowerTalk] KT34XA cracked insulators
To: <towertalk@contesting.com>
> Date: Tuesday, May 06, 1997 6:26 AM
> 
> Polycarbonate resins, such as GE LEXAN and others, are extremely
> susceptable to solvents such as WD-40.  The GE book lists these chemicals
> to avoid:
> 
> Amines, Aromatic Hydrocarbons, strong alkaline detergents, Esters,
> Halogenated Hydrocarbons, Ketones.
> 
> Also avoid the following combination:  High stress, Hot water, High
> temperature (140-160 deg F).
> 
> It is really amazing to see the effects of these chemicals on a sample
> part.  Extreme crazing and cracking in a matter of seconds!
> 
> Roger WB0DGF

--
FAQ on WWW:               http://www.contesting.com/towertalkfaq.html
Submissions:              towertalk@contesting.com
Administrative requests:  towertalk-REQUEST@contesting.com
Problems:                 owner-towertalk@contesting.com

<Prev in Thread] Current Thread [Next in Thread>