If you are using the tradition "shots" the starting powder is compacted at
the bottom of the tube. You'll need to tap on the tube after you've poured
the weld metal out so the starting material gets loosen enough for you to
sprinkle on top of the weld metal and to the side of the mold. If you've had
these shots for a long time already, 2 things might have happened. 1 -
You've shaken the tubes (Shots) too much that the starting material got
completely mixed in with the weld metal. In that case, there's no way for
you to ignite it. You'll have to buy new shots for it. 2 - If you had these
tubes for a long time, 20% of the time they are lost due to moisture issues.
Again there's nothing you can do about it except to go buy new shots.

If you are using the Foil Pack type weld metals, the starting materials are
in it's own separate containers and all you have to do is open that and
sprinkle some on top of the weld metal and side of the mold. 

I don't recommend you to light the starting materials with a torch since
it's most likely not going to be hot enough to light it up. All you'll end
up doing is blowing the starting material all over the place from the
pressure by the torch. The starting material lights up at 800 degrees. And
the Weld Metal reacts at 1800 degrees. Then the whole exothermic reaction
burns at 4300 degrees. For this reason, I strongly suggest you to only
ignite the starting material with a "Flint Ignitor". 

If you have any questions, feel free to call me at anytime or visit our
website at www.atitec.com for more information. I hope this is helpful for
you!

Wilson Lui
ATI Tectoniks
Tel: +1(310) 257-1616
        +1(877) EXOWELD
Fax: +1(310) 257-1170

wilsonlui@atitec.com



Please visit our website at http://www.atitec.com for more information.


-----Original Message-----
From: towertalk-bounces@contesting.com
[mailto:towertalk-bounces@contesting.com] On Behalf Of Howard Klein
Sent: Monday, May 24, 2004 1:56 PM
To: towertalk@contesting.com
Subject: [TowerTalk] Cadweld help

Is the starting powder for the Cadweld combined with the welding metal or is

it separate? I ran the gamut of a spark igniter to a  propane torch. The 
powder glowed red but no exothermic reaction. What am I doing wrong?
Howard...K2HK


_______________________________________________

See: http://www.mscomputer.com  for "Self Supporting Towers", "Wireless
Weather Stations", and lot's more.  Call Toll Free, 1-800-333-9041 with any
questions and ask for Sherman, W2FLA.

_______________________________________________
TowerTalk mailing list
TowerTalk@contesting.com
http://lists.contesting.com/mailman/listinfo/towertalk


_______________________________________________

See: http://www.mscomputer.com  for "Self Supporting Towers", "Wireless Weather 
Stations", and lot's more.  Call Toll Free, 1-800-333-9041 with any questions 
and ask for Sherman, W2FLA.

_______________________________________________
TowerTalk mailing list
TowerTalk@contesting.com
http://lists.contesting.com/mailman/listinfo/towertalk

<Prev in Thread] Current Thread [Next in Thread>