I have to use you folks for a technical question.  18.8ss or 304ss?

The supplier suggested these two grade types.

 

Is there any difference, how much?  

 

They will be used on a force 12 XR5 refurbish and a rotor plate
attachment.  

 

He stated that the u-bolts will not be submerged in salt water, but in a
salt water environment and that either grade would suffice.  Tampa Bay
is out the back door and if a piece of steel sits out for a few days
will rust up quite nicely.  I have several pliers that attest to this
conclusion.  

 

The vertical works quite nicely in this environment though!  I guess a
decent trade off.

 

Any thought?

 

Thanks to all that have assisted me to this point.

 

D 'Noid' Wilson

Frontline Communication

"The Finest Command and Broadcast Vehicles in the World"

BAS 2 GHz Relocation Project ENG

727.580.8603

727.571.3295 FAX

Semper Fi

dwilson@frontlinecomm.com <mailto:dwilson@frontlinecomm.com> 

dwilson@oshkoshsv.com

dwilson@aksv.com

 

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email 
______________________________________________________________________
_______________________________________________



_______________________________________________
TowerTalk mailing list
TowerTalk@contesting.com
http://lists.contesting.com/mailman/listinfo/towertalk

<Prev in Thread] Current Thread [Next in Thread>