>>First of all, wear gloves! This stuff is nasty! Stinks to all high heaven
>>too.  It took about 1/2 hour of mixing to dissolve the zinc solids in the
>>paint, and even then, you can never get it completely stirred.
>
>I liberated one of my wife's wooden spoons and put it into the end of my
>drill.  It will mix it up very
>thouroughly and with minumum effort!
>
>73...Scott K8DX
___________________________________________________________________________
That settles it!  I'm going to stick to Cold Galvanizing by LPS.  It is only
$6 + change for a 16 oz. spray can that covers quite a bit of area.... and
it is 95% zinc!

Rod, N5HV
w5hvv@aeneas.net



--
FAQ on WWW:               http://www.contesting.com/towertalkfaq.html
Submissions:              towertalk@contesting.com
Administrative requests:  towertalk-REQUEST@contesting.com
Problems:                 owner-towertalk@contesting.com
Search:                   http://www.contesting.com/km9p/search