[Towertalk] mast strength
W0UN--John Brosnahan
shr@ricc.net
Tue, 24 Dec 2002 13:55:38 -0600
At 01:18 PM 12/24/2002 -0600, Paul DeWitte K9OT wrote:
>Since schedule 80 is twice as thich as schedule 40 they are not the same
>strength.
Yield strength is a materials spec. Both Schedule 80 and 40 are the
same material--so their material yield strength is the same. But the
actual load they can handle is a function not only of the material yield
strength but also the wall thickness and diameter. You need all three
to calculate the capabilty of a mast.