[TowerTalk] C-4XL tubing wall thicknesses

Pete Smith n4zr at contesting.com
Sun Aug 10 14:41:50 EDT 2003


At 12:46 PM 8/10/03 -0400, you wrote:
>>>What are the wall thicknesses of the tubing in the elements of a Force 
>>>12 C-4XL, for
>>>
>>>* the standard, 80-mph, model;
>>>* the "D," 100-mph, model;
>>>* the "H," 120-mph, model; and/or
>>>* the "HH," 140-mph, model ?
>>
>>Perhaps an F-12 person will comment, but I believe they all use the 
>>standard wall, which permits telescoping in 1/8 inch increments;  I 
>>believe they beef up by doubling and tripling the critical sections.
>
>What is "the standard wall"?  For zero clearance, it'd be 1/16th inch, or 
>0.0625".  So, is 0.058, which would leave 0.0045", the standard?  (I guess.)

I am pretty sure that's right.

73, Pete N4ZR