I have not been too impressed with "cold galvanising".  I found that it 
begins to rust through after a year or two.  I have had much better results 
with Rustoleum "rusty metal" aluminium paint.  It seems to last almost as 
long as real galvanising.  My Rohn 25 tower has been up for over 25 years.  
I use an ex-AMBC tower base insulator with ungalvanised iron castings bonded 
to each end of the ceramic, and an ungalvanised steel adaptor plate to 
attach the insulator to the bottom of the tower.  I painted the end castings 
and adaptor plate with the Rustoleum, and I think I have repainted it once, 
and it is still in good shape, while the tower itself is beginning to show 
quite a bit of rust on the surface.

The Rustoleum soaks into surface rust and fills the pores, so that the 
paint-saturated rust acts like a primer and makes the coat of paint adhere 
more tightly than it would to bare metal.

Don k4kyv

_________________________________________________________________
Get FREE Web site and company branded e-mail from Microsoft Office Live 
http://clk.atdmt.com/MRT/go/mcrssaub0050001411mrt/direct/01/



More information about the TowerTalk mailing list