>> Stay-Brite (at least some of them) is a Low temp silver bearing solder,
> that (at least with the rolls I have) melts at temps BELOW what normal
> 60/40 melts at (does anyone actually use 60/40?  I always use 63/37 for
> electronics, but that's me)

Actually, it melts about 100 degrees higher than tin/lead.
Stay Brite is 96% tin, 4% silver, no lead.

Rick N6RK