I just completed hand painting four 20 foot sections of tower.  The
hot dip galvanizing was beginning to show some rust and I learn that
the cold galvanizing spray cans were too expensive.   I was provided
information from a commercial paint company that sells product to tank
and structural steel folks.

Devoe Coatings, Louisville, KY
Devguard 4160- Multi-Purpose Tank and Structural Primer

Comes in Gray or White.

It  brushed on nicely.   I found that it didn't really need to be
stirred as do other paints.  This is a very thick paint, and the tower
took 3/4 of a gallon.  Not easy painting, but the price was 31.00 per
gallon.  It must be used in a temp of 50 degrees or over.

George Clute - W7LFD





List Sponsor:  ChampionRadio.com - Trylon self-supporting towers,
safety equipment, rigging gear, LOOS tension guages & more!
http://www.championradio.com

-----
FAQ on WWW:               http://www.contesting.com/FAQ/towertalk
Submissions:              towertalk@contesting.com
Administrative requests:  towertalk-REQUEST@contesting.com
Problems:                 owner-towertalk@contesting.com


<Prev in Thread] Current Thread [Next in Thread>