[Amps] Burn-in for GU84b?
Carl
km1h at jeremy.mv.com
Mon Nov 18 09:43:28 EST 2013
I dont know the gettering process of Russian tubes, or the official "burning
in" procedure of long stored tubes, but if it is the same as indirectly
heated US ceramic/metal tubes then running just the filaments for 24 hours
would be the way to go.
Carl
KM1H
----- Original Message -----
From: "Rich Hallman - N7TR" <rich at n7tr.com>
To: <amps at contesting.com>
Sent: Sunday, November 17, 2013 10:45 PM
Subject: [Amps] Burn-in for GU84b?
> Is there a process to burn in a new GU84 tube?
> Thanks..
> Rich N7TR
> ex KI3V, N3AMK, WB3JOV
> www.n7tr.com<http://www.n7tr.com>
> http://www.qrz.com/db/N7TR
> Telnet: dxc.n7tr.com N7TR DXCluster
>
>
> _______________________________________________
> Amps mailing list
> Amps at contesting.com
> http://lists.contesting.com/mailman/listinfo/amps
>
>
> -----
> No virus found in this message.
> Checked by AVG - www.avg.com
> Version: 10.0.1432 / Virus Database: 3222/6346 - Release Date: 11/18/13
>
More information about the Amps
mailing list