[Amps] Cool Amp Silver Plating

MU 4CX250B 4cx250b at miamioh.edu
Fri Feb 28 10:48:29 EST 2014


I've used Cool-Amp powder for many years. It works fine, is easy to
use. Seems non-toxic, although I always wear gloves. No ventilation
needed. I think the coating is thinner electroplated silver.
73,
Jim w8ZR

Sent from my iPhone

> On Feb 28, 2014, at 8:27 AM, "Fuqua, Bill L" <wlfuqu00 at uky.edu> wrote:
>
> Take a look at this.
> http://www.saltlakemetals.com/SilverChloridePlating1.htm
> 73
> Bill wa4lav
>
> ________________________________________
> From: Amps [amps-bounces at contesting.com] on behalf of Hardy Landskov [n7rt at cox.net]
> Sent: Friday, February 28, 2014 9:42 AM
> To: amps at contesting.com
> Subject: [Amps] Cool Amp Silver Plating
>
> All,
> Has anyone used this power? If so, what is your opinion/facts of how your project turned out? Any special precautions needed?
> Thanks ahead of time.
> 73 Hardy N7RT
> _______________________________________________
> Amps mailing list
> Amps at contesting.com
> http://lists.contesting.com/mailman/listinfo/amps
> _______________________________________________
> Amps mailing list
> Amps at contesting.com
> http://lists.contesting.com/mailman/listinfo/amps


More information about the Amps mailing list