> I have been told totally opposite approaches for treating 4130 Chrome-
> moly mast material. I'd like to learn what others have done. So what
> is recommended ?
I'm not sure what you mean by "totally opposite approaches".
In general, some sort of protective coating will eliminate or retard
oxidation. The best is hot-dipped galvanizing. If that's impractical, then
using some sort of manually applied coating will work. This could be an
industrial coating or marine paint.
I don't know what the rate of oxidation is on a piece of chromoly steel,
but even untreated it'd probably last for 50 years or more.
Cheers, Steve K7LXC
--
FAQ on WWW: http://www.contesting.com/towertalkfaq.html
Submissions: towertalk@contesting.com
Administrative requests: towertalk-REQUEST@contesting.com
Problems: owner-towertalk@contesting.com
Search: http://www.contesting.com/km9p/search.htm