[TowerTalk] Old KLM Paste
Ted Leaf
tleaf@hotmail.com
Tue, 27 Jun 2000 00:36:43 HST
Hi Bill,
Two years ago when I bought my KT-34A, It came with the grey zinc paste. I
don't know who they got it from or if they made it them self.
I myself, won't use cooper paste with aluminum.
73, Aloha
Ted Leaf, K6HI
Kona, Hawaii
<tleaf@hotmail.com>
-----------------
Date: Mon, 26 Jun 2000 13:05:55 -0400
From: wbh3@daimlerchrysler.com
Subject: Re: [TowerTalk] Antenna Grease--Deficiencies and
Remedies
FWIW when I built my kt34-xa about 7 years ago, KLM supplied a
little can
of copper-colored paste to put on the joints. After a move
and whenn I
was reassembling the end units I found this paste had turned
very solid and
seemed to be a good insulator as the resistance checks I made on
each
element end were very high. Don't know what KLM used but I
don't think it
was very good stuff.
Bill Haselmire WX8S
------------------------------
________________________________________________________________________
Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com
--
FAQ on WWW: http://www.contesting.com/FAQ/towertalk
Submissions: towertalk@contesting.com
Administrative requests: towertalk-REQUEST@contesting.com
Problems: owner-towertalk@contesting.com