[TowerTalk] Cold Galvanizing Spray
Steve Maki
steve@oakcom.com
Mon, 30 Jul 2001 12:46:27 -0400
WS6X wrote:
>I am intrigued by the glowing TT comments regarding cold galvanizing spray. Since my experience is so much to the contrary, I must be “Ralphing up” the process somehow. I’m hoping someone here can correct the error of my ways.
>
>I have tried 3 different brands. I have enthusiastically read all the promo stuff: “Rich with self-sacrificing zinc, creating a durable bond, etc., etc.”
>
>I have applied the spray paint directly over clean, existing galvanized steel. I have applied it to new, buffed (with steel wool, and/or emery cloth) steel, and to chemically etched, new steel. I have allowed it to “cure” for 12 weeks. I have yet to achieve what I would consider a “bond.” To wit: the paint can be scraped off down to original surface with the slightest effort. In fact I can even rub it off with a callus on my thumb!
>
>What am I missing?
>
>Thanks,
>
>Jim - WS6X
You only tried three brands? :-) I tried a dozen or so before
finding a good one.
Try "Brite Zinc".
It's leaves the hardest, best looking finish I've seen.
--
Steve K8LX
-----