I've had good luck removing oxidation from normal stranded hard-drawn copper wire using a product called "Copper Glo Liquid". http://barkeepersfriend.com/copper%20glo.htm On wire that has been exposed to the elements for years it takes awhile to work and more than one application may be required. I've never tried it on flex-weave. 73, John, K9MM _______________________________________________ _______________________________________________ TowerTalk mailing list TowerTalk@contesting.com http://lists.contesting.com/mailman/listinfo/towertalk |
<Prev in Thread] | Current Thread | [Next in Thread> |
---|---|---|
|
Previous by Date: | Re: [TowerTalk] Drilling tubing (180 deg), Doug Faunt N6TQS +1-510-655-8604 |
---|---|
Next by Date: | Re: [TowerTalk] Drilling tubing (180 deg), Jim Miller |
Previous by Thread: | Re: [TowerTalk] Soldering flex-weave, WA3GIN |
Next by Thread: | [TowerTalk] cleaning Flexweave, Craig Clark |
Indexes: | [Date] [Thread] [Top] [All Lists] |