It is a flash plating and is very thin. If you polish it to look shiny
you can easily polish it right off to the base metal, so it is extremely
thin. probably no more than a few microns thick. Easy to use on open
surfaces and a PITA to do coils. Better to do the tubing and then wind
the coil.
IIRC no special tools or precautions are necessary other than common
sense. NOTE. I used a lot of it, but it was in my early days as an
instrument tech. (early 1960's so take with a grain of salt) I also did
a lot of silver plating with both cyanide (smooth coat) and
nitrates(rough coat)
Electroplating works much better, but the chemicals are dangerous.
(silver cyanide) Can give off cyanide. Wear chemical gloves and face
shield and do in a fume hood, or properly ventilated area.
_______________________________________________
Amps mailing list
Amps@contesting.com
http://lists.contesting.com/mailman/listinfo/amps
_______________________________________________
Amps mailing list
Amps@contesting.com
http://lists.contesting.com/mailman/listinfo/amps
|